Group Company of Vicat, France
|
|
|
|
|
|
OPC 43 Grade
|
Ordinary Portland Cement 43 grade is manufactured by inter grinding of high grade clinker (with optimum C3Scontent) and right quality gypsum in appropriate proportions. |
|
|

|
|
|
Properties
a) Physical |
Requirements as per
IS 8112-1989 |
Bharathi cement
values |
Competitors values |
| Fineness (sqm/kg) |
225(min) |
325 |
280 |
|
Soundness (mm) |
| Lechatlier method |
10mm (max) |
1 |
1.5 |
| Autoclave (%) |
0.8 (max) |
0.03 |
0.05 |
|
Setting time |
| Initial (min) |
30 minutes |
150 |
280 |
| Final (max) |
600 minutes |
260 |
340 |
|
Compressive strength (MPa) |
| 1 day |
|
17 |
14 |
| 3 days (min) |
23 |
35 |
30 |
| 7 days (min) |
33 |
45 |
40 |
| 28days (min) |
43 |
63 |
51 |
| b) Chemical |
| 1) Lime saturation factor |
0.6-1.02 |
0.9 |
0.8 |
| 2) Alumina Modulus |
0.66 (min) |
1.23 |
1.24 |
| 3)Insoluble residue (%) |
3 (max) |
0.25 |
1.5 |
| 4)Magnesia (%) |
6 (max) |
1 |
1.02 |
| 5)Sulphuric anhydrideSO3 (%) |
3 (max) |
1.5 |
2.3 |
| 6)Loss on ignition (%) |
5 (max) |
0.8 |
1.5 |
| 7)Alkalies |
|
|
0.6 |
| 8) Chloride (%) |
0.1 (max) |
0.002 |
0.02 |
| 9) C3A Content |
|
7 |
|
| 10)Temperature during Testing |
27±2 |
27±2 |
27±2 |
| 11)Humidity (%) |
65±5 |
65±5 |
65±5 |
|
|
| APPLICATIONS: |
-
All types of R.C.C.works
-
Residential and commercial complexes
-
Industrial structures
-
Bridges, dams, irrigation works
-
For highways, runways etc.
|
|
|

|
|